Before Picture
Before
After Picture
After

Cleaning Trial Summary

 

The customer was looking to improve their cleaning performance.

Cleaning Trial Type
Temperature
Polymer
150°F
Industry
Time Required
Polymer Manufacturing
10 hours
Segment
Substrate
Non-metal Manufacturing
Stainless Steel, Steel
Soil
Polyuria
Description of Part(s)
Pipe
Cleaner Used
Machine Used

Agitating Immersion Washer (SK 81.8, Graymills T12, Graymills T24)

Post Cleaning

Fresh water rinse followed by air pressure drying.

Recommendation to Customer

 The ArmaKleen Technical Center recommended using 100% by volume ArmaKleen™ Paint and Ink Remover at 150°F in an Agitating Immersion Washer for a minimum of 10 hours.