Before
After

Cleaning Trial Summary

 

Improve cleaning performance, reduce rework and reject rate, and automate cleaning process

Cleaning Trial Type
Temperature
Ink
160°F
Industry
Time Required
Packaging
8 hours
Segment
Substrate
Fabricated Metal Product
Stainless Steel
Soil
Ink (Flexographic), Ink (UV)
Description of Part(s)
Die/dispensers
Cleaner Used
Machine Used

Spray Under Immersion Washer (SK Model 81.8, Graymills T12, Graymills T24 w/ SUI), Ultrasonic Washer (SK Blackstone 6315)

Post Cleaning

Fresh water rinse and air pressure drying

Recommendation to Customer

The ArmaKleen Technical Center recommends using a 100% by volume solution of ArmaKleen™ Paint and Ink Remover at 160°F in a Spray-Under Immersion Washer or an Ultrasonic Washer for a minimum of 8+ hours