Before
After

Cleaning Trial Summary

 

The customer was looking to improve their cleaning performance, automate their cleaning process, clean mixed metals together and eliminate hazardous chemicals/waste.

Cleaning Trial Type
Temperature
Aqueous
160°F
Industry
Time Required
Firearm sling manufacturer
15 – 30 minutes
Segment
Substrate
Fabricated Metal Product
Aluminum, Brass, Copper, Plastic, Stainless Steel, Steel
Soil
Cutting Fluids, Oil
Description of Part(s)
an assortment of machine parts
Cleaner Used

• 10% by volume ARMAKLEEN™ M-HP-2

• 10% by volume ARMAKLEEN™ MM-Recycle

Machine Used

Ultrasonic Washer (SK Blackstone model 6315)

Post Cleaning

Fresh water rinse and air pressure dried.  Parts were then placed in an oven at 210°F for 30 minutes.

Recommendation to Customer

The ArmaKleen Technical Center recommends using a 10% by volume solution of ArmaKleen™ M-HP-2 at 160°F in an Ultrasonic Washer or a 10% by volume solution of ArmaKleen™ MM-Recycle at 160°F in an Ultrasonic Washer for a minimum of 15-30 minutes.